TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0N-330 Black20.0Sulfur1.5THANECURE® ZM1.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
Tensile Strength, Yield 26.3 MPa
3810 psi
Elongation at Yield 487 %
487 %
100% Modulus 0.00259 GPa
0.375 ksi
200% Modulus 0.00636 GPa
0.922 ksi
300% Modulus 0.01194 GPa
1.732 ksi
Tear Strength 35.9 kN/m
205 pli
Die C
Processing Properties Metric English Comments
Cure Time 9.00 min

@Temperature 177 °C
0.150 hour

@Temperature 350 °F