Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Sulfur Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Sulfur Cure.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5TP-9510.0N-330 Black51.0AC Poly 617A1.5MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Yield 24.12 MPa
3499 psi
Elongation at Yield 495 %
495 %
100% Modulus 0.00560 GPa
0.812 ksi
200% Modulus 0.01193 GPa
1.731 ksi
300% Modulus 0.01739 GPa
2.522 ksi
Tear Strength 63.9 kN/m
365 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 155 °C
0.250 hour

@Temperature 311 °F