Struktol V-MAT G Processing Additive, Matting Agent

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol V-MAT G Processing Additive, Matting Agent.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A mixture of additives and light-colored aliphatic resins with a molecular weight below 2,000.STRUKTOL® V-MAT G is highly effective for matting and texture of rigid PVC. STRUKTOL® V-MAT G can be used at relatively high loading levels without significantly changing the fusion characteristics of the compound. Ideal for water channeling profile applications. The benefits of STRUKTOL®V-MAT G include matting surface effect, minimum fusion effect and textured surface.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
Additive Loading 2.0 - 5.0 %
2.0 - 5.0 %
Ash 21 %
21 %
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Yellow to white powder