Struktol TPW 604 Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TPW 604 Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
STRUKTOL® TPW 604 is a blend of lubricants designed specifically for wood fiber/flour filled polyolefins. This product will provide improved surface quality, increased output rates and a wider processing window leading to overall improved processability.Applications: STRUKTOL® TPW 604 can also be used in other polyolefin compounds where improved processability or output rates are required.Information provided by Struktol
Physical Properties Metric English Comments
Additive Loading 2.0 - 7.0 %
2.0 - 7.0 %
Thermal Properties Metric English Comments
Dropping Point 95.0 - 113 °C
203 - 235 °F
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Off-white to light tan pastille or bead