Material Notes:
Application: Molding for solesInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.257 g/cc
0.04541 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength at Break 14.61 MPa
2119 psi
ISO R 527
Elongation at Break 352 %
352 %
ISO R 527
Abrasion 155
155
mm³; ISO 4649