Crucible Steel AISI 8620 Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel , AISI 8000 Series Steel
Manufacturer Crucible Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel AISI 8620 Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Crucible Industries
Physical Properties Metric English Comments
Density 7.83 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 143 - 163
143 - 163
Modulus of Elasticity 207 GPa
30000 ksi
Component Elements Properties Metric English Comments
Carbon, C 0.20 %
0.20 %
Chromium, Cr 0.50 %
0.50 %
Iron, Fe 97.45 %
97.45 %
as balance
Manganese, Mn 0.80 %
0.80 %
Molybdenum, Mo 0.20 %
0.20 %
Nickel, Ni 0.55 %
0.55 %
Silicon, Si 0.30 %
0.30 %