Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Stellar Canada CERAMITE® CSR-F Wear Resistant Castable

Category Ceramic , Carbide
Manufacturer Stellar Canada
Trade Name CERAMITE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Stellar Canada CERAMITE® CSR-F Wear Resistant Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world wide, both as mortars and as various precast components. Ceramite can easily be mixed, cast and shaped in any size and is thus comfortably to work with in-situ. Ceramite can be used in within a wide range of temperatures and applications exposed to thermal shock conditions in industries like for example aluminum, cement and ferro.Applications: Floor Tile, Hearth/Furnace Tile, Furnace Sills & Doors, Lintels, Pipe and Duct Linings, Feed Tubes, Troughs/Launders, Ladles, Dampers, Nozzle Blasters, Crucible Linings, Vortex, Burner Tip Cooler Plates, Nose Ring, Electrical Insulation, Cold Wear AreasSpecific Notes on This Grade: A trowelable formulation with extreme abrasion resistance and high thermal conductivity. Used in the same industries as BKR in areas with high abrasion problems. References as lining material for pipes and bends, lining of transportation systems, duct linings etc...Information provided by Stellar Canada.
Physical Properties Metric English Comments
Bulk Density 2.69 g/cc
0.0972 lb/in³
Trowellable
Mechanical Properties Metric English Comments
Modulus of Rupture 0.02100 GPa
3.046 ksi
Hot, prefired at 1832°F/24 hours (1000°C)
Flexural Strength 10.88 MPa
<br>@Temperature 1200 °C
1578 psi
<br>@Temperature 2192 °F
after Firing; ASTM-349
12.30 MPa
<br>@Temperature 500 °C
1784 psi
<br>@Temperature 932 °F
after Firing; ASTM-349
15.30 MPa
<br>@Temperature 850.0 °C
2219 psi
<br>@Temperature 1562 °F
after Firing; ASTM-349
17.90 MPa
<br>@Temperature 1000 °C
2596 psi
<br>@Temperature 1832 °F
after Firing; ASTM-349
Compressive Strength 71.002 MPa
<br>@Temperature 1200 °C
10298 psi
<br>@Temperature 2190 °F
after Firing; ASTM C-349
108.00 MPa
<br>@Temperature 1000 °C
15664 psi
<br>@Temperature 1830 °F
after Firing; ASTM C-349
114.00 MPa
<br>@Temperature 850 °C
16535 psi
<br>@Temperature 1560 °F
after Firing; ASTM C-349
150.00 MPa
<br>@Temperature 500 °C
21756 psi
<br>@Temperature 932 °F
after Firing; ASTM C-349
157.00 MPa
<br>@Temperature 20.0 °C
22771 psi
<br>@Temperature 68.0 °F
after 7 days
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1000 °C
1832 °F
Component Elements Properties Metric English Comments
Al2O3 18 %
18 %
CaO 7.1 %
7.1 %
Fe2O3 0.040 %
0.040 %
K2O 0.020 %
0.020 %
MgO 0.010 %
0.010 %
Na2O 0.010 %
0.010 %
SiC 64 %
64 %
SiO2 10 %
10 %
Descriptive Properties Value Comments
Application Troweling
Copyright © lookpolymers.com All Rights Reserved