Solvay Specialty Polymers Virantage® VW-10700 RP, RFP, RSFP Polyethersulfone (PESU)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer Solvay Specialty Polymers
Trade Name Virantage®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Virantage® VW-10700 RP, RFP, RSFP Polyethersulfone (PESU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial properties in epoxy thermosets. Their inherent toughness imparts damage tolerance to thermoset composites and excellent flexibility to coatings. Virantage® polymers also offer superior thermal and hydrolytic stability that delivers best-in-class hot-wet performance.Features: Amorphous; Good Thermal Stability; Good Toughness; High Heat Resistance; Hydrolytically Stable; Low Molecular Weight; Low ViscosityUses: Aerospace ApplicationsAdditional Properties: Average Molecular Weight - Internal Method 21000 g/mol; Moisture - Internal Method 1.5 %; OH End Groups - Internal Method 210 µeq/g; Particle Size - 75.0 µm; Particle Size - 500 µm; Particle Size - 45.0 µm; Residual Solvent - Internal Method 0.15 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Viscosity 560 cP
560 cP
Solution Viscosity; ASTM D455
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 216 °C
421 °F
ASTM E1356
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Coating; Compounding