Material Notes:
Veradel A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water and mineral acids. Cast films or coatings of PESU are transparent and have additional desirable properties including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance. Typical applications include high-temperature coating formulations, advanced high-temperature composites and specialty adhesives. Veradel A-704P is relatively low in molecular weight and viscosity. A higher molecular weight and viscosity grade is available as A-304P. This grade was formerly marketed as Radel® A PESU - Natural: Veradel A-704P NTInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Viscosity 200 cP

@Temperature 40.0 °C
200 cP

@Temperature 104 °F
Solution, 25% in Dimethylacetamide; Internal Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.0 µm/m-°C
27.2 µin/in-°F
ASTM D696
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Appearance Transparent - Slight Yellow
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Acid Resistant
Flame Retardant
Food Contact Acceptable
Good Adhesion
Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Thermal Stability
Good Toughness
High Flow
High Heat Resistance
High Tensile Strength
Hydrolysis Resistant
Low Molecular Weight
Medium Rigidity
Forms Powder
Generic PESU
Processing Method Coating
Solution Processing
Spraying
Residual Solvent (%) 0.50
Internal Method
RoHS Compliance RoHS Compliant
Uses Adhesives
Coating Applications
Copyright © lookpolymers.com All Rights Reserved