Solvay Specialty Polymers Torlon® AI-10 LM Polyamide-imide (PAI)

Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Extruded
Manufacturer Solvay Specialty Polymers
Trade Name Torlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Torlon® AI-10 LM Polyamide-imide (PAI).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Torlon® AI-10 LM is a polyamide-imide (PAI) powder developed for the performance coatings industry. It is similar to Torlon® AI-10 in that it is produced using the same monomers and polymerization system. However, the manufacturing process has been optimized to reduce the amount of residual methylene dianiline (MDA) monomer to below the 1000 ppm action level specified in various hazard communication regulations.Torlon® AI-10 LM can be substituted for Torlon® AI-10, without any changes in formulation or process. Coatings based on the Torlon® AI-10 or AI-10 LM polymer yield durable, abrasion resistant, thermally stable films. The resin has superior resistance to organic solvents and a wide array of other commercial and industrial chemicals.Features: Flame Retardant; Good Abrasion Resistance; Good Adhesion; Good Chemical Resistance; High Heat Resistance; Water SolubleUses: Binder; Coating ApplicationsAdditional Properties: Acid Number - 82.00 mg KOH/g; Solids Content - 92 %; Viscosity - (23°C): 850 mPa·sInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Yellow
Form Powder
Processing Technique Coating; Solution Processing