Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide (PPS)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS); Molded
Manufacturer Solvay Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide (PPS).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ryton® Polyphenylene Sulfide (PPS) resins are available in several grades exhibiting different molecular weights and molecular architecture. Ryton® PPS exhibits excellent thermal stability and chemical resistance and is suitable for a variety of applications including coatings, compounds, and extrusion.Features: Good Chemical Resistance; Good Thermal StabilityUses: Coating Applications; CompoundingAdditional Properties: Ash Content - 0.8 wt%Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Melt Flow 5000 g/10 min

@Load 5.00 kg,
Temperature 315 °C
5000 g/10 min

@Load 11.0 lb,
Temperature 599 °F
Procedure B; ASTM D1238
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Off-White
Form Powder
Processing Technique Coating; Compounding; Extrusion; Extrusion Coating
RoHS Compliance RoHS Compliant