Material Notes:
Polymist® XPP 538 a white PTFE micronized powder PTFE micronized powder composed of discrete particles. Designed for use in critical engineering and high end performance coatings and inks, Polymist® XPP 538 will improved non-stick properties and mar and abrasion resistance as well as slip and rub resistance.Uses: AdditiveAdditional Properties: Bulk Density - ASTM D4895 400 g/l; Grind in Oil - NPIRI 2.50; Melt Temperature - ASTM D3418 320 to 330 °C; Particle Size - Internal Method 15.0 µm; Particle Size - Internal Method 4.50 µm; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder