Material Notes:
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, inherent flame resistance, low surface energy, and exceptional dielectric properties. Hyflon® PFA resins have been designed to retain their properties over a wide range of temperatures from cryogenic to 250-260°C (482-500°F) and are the material of choice in applications such as linings in the Chemical Process Industry, specialty cables, semiconductor industry, aerospace, and other challenging industries.Hyflon® PFA 220X is a low melt flow rate resin designed for blow molding applications, where very high viscosity and melt strength are needed. It also has significantly lower permeability to gasses than standard PFAs.Features: Flame Retardant; High Heat Resistance; Low Flow; Semi CrystallineUses: Aerospace Applications; Cable Jacketing; Liners; Piping; Semiconductor Molding Compounds; TubingAdditional Properties: Crystallization Heat - DSC 35.0 to 45.0 J/g; Density - ASTM D792 2.120 to 2.170 g/cm³; Heat of Fusion - DSC 35.0 to 45.0 Jg; Linear Expansion Coefficient - ASTM D696 1.2E-4 to 2.0E-4 cm/cm/°C; Melt Flow - ASTM D1238 2.50 to 5.00 g/10 min; Tensile Modulus - ASTM D1708 (280°C): 49.0 MPa; Tensile Strength at Break - ASTM D1708 (280°C): 4.60 MPaInformation provided by Solvay Specialty Polymers.
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D638
Elongation at Break >= 210 %
>= 210 %
ASTM D638
Tensile Modulus 0.600 GPa
87.0 ksi
ASTM D638
Thermal Properties Metric English Comments
Specific Heat Capacity 0.900 - 1.10 J/g-°C
0.215 - 0.263 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.200 W/m-K

@Temperature 40.0 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 104 °F
ASTM C177
Melting Point 309 - 312 °C
588 - 594 °F
DSC
Crystallization Temperature 295 °C
563 °F
Peak; ASTM D3418
Descriptive Properties Value Comments
Agency Ratings ASTM D 3307 Type II
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Extrusion