Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Solvay Specialty Polymers
Trade Name Hyflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, inherent flame resistance, low surface energy, and exceptional dielectric properties. Hyflon® PFA resins have been designed to retain their properties over a wide range of temperatures from cryogenic to 300°C (572°F)* and are the material of choice in applications such as linings in the chemical process industry, specialty cables, semiconductor industry, aerospace, and other challenging industries. Hyflon® PFA 125 is a low melt flow rate perfluoroalkoxy resin designed for enhanced creep resistance, higher long-term pressure resistance, and excellent thermal stability. It is a Type II PFA according to ASTM D 3307.Features: Flame Retardant; High Heat Resistance; Low Flow; Semi CrystallineUses: Aerospace Applications; Cable Jacketing; Liners; Piping; Semiconductor Molding Compounds; TubingAdditional Properties: Crystallization Heat - ASTM D4591 28.0 to 38.0 J/g; Density - ASTM D792 2.120 to 2.170 g/cm³; Heat of Fusion - ASTM D4591 28.0 to 38.0 J/g; Linear Expansion Coefficient - ASTM D696 1.2E-4 to 2.0E-4 cm/cm/°CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Melt Flow 1.5 - 3.0 g/10 min

@Load 5.00 kg,
Temperature 372 °C
1.5 - 3.0 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
ISO 868
Tensile Strength at Break >= 25.0 MPa
>= 3630 psi
ASTM D638
4.60 MPa

@Temperature 280 °C
667 psi

@Temperature 536 °F
ASTM D1708
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Specific Heat Capacity 0.900 - 1.10 J/g-°C
0.215 - 0.263 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.150 - 0.250 W/m-K

@Temperature 40.0 °C
1.04 - 1.74 BTU-in/hr-ft²-°F

@Temperature 104 °F
ASTM C177
Melting Point 310 - 316 °C
590 - 601 °F
DSC
Crystallization Temperature 285 - 295 °C
545 - 563 °F
Peak; ASTM D3418
Oxygen Index 95 %
95 %
ASTM D2863
Descriptive Properties Value Comments
Agency Ratings ASTM D 3307 Type II
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Extrusion