Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers FOMBLIN® LC200 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® LC200 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requiring low viscosity.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
ASTM D891
Viscosity Measurement 122
122
Viscosity Index; ASTM D2270
Kinematic Viscosity 190 cSt

@Temperature 20.0 °C
190 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 65.6 cSt
65.6 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 9.4 cSt
9.4 cSt
ASTM D445
Molecular Weight 2900 g/mol
2900 g/mol
Evaporation Loss 1.7 %
1.7 %
22 hrs. at 60°C; ASTM 2595
17 %
17 %
22 hrs. at 120°C; ASTM 2595
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 105 kg
232 lb (mass)
Mean Hertz Load; IP 239
400 kg
882 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.700 mm
0.0276 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -40.0 °C
-40.0 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 68
Oxygen Impact (BAM) 100°C, Impact Pressure 180 atm