Description: Rhodiasolv PolarClean is a eco-friendly water soluble polar solvent or co-solvent very effective to solubilize agrochemicals. It is recommended to use in EC’s (emulsifiable concentrate) at 20 to 60 %. In addition to its high solvency property, Rhodiasolv PolarClean acts also as crystal growth inhibitor and improves the cold stability of your final formulationIdentification: METHYL-5-(DIMETHYLAMINO)-2-METHYL-5-OXOPENTANOATECAS: 1174627 – 68 – 9Available in: Asia Pacific, Europe, Latin America and North America Solubility at 23°C – 50/50 v/v in water: Miscible Applications: Rhodiasolv PolarClean is a eco-friendly water soluble polar solvent or co-solvent very effective to solubilize agrochemicals. It is recommended to use in EC’s (emulsifiable concentrate) at 20 to 60 %. In addition to its high solvency property, Rhodiasolv PolarClean acts also as crystal growth inhibitor and improves the cold stability of the final formulation.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.0147 - 1.0149 g/cc
0.036658 - 0.036666 lb/in³
Thermal Properties Metric English Comments
Melting Point <= -60.0 °C
<= -76.0 °F
Freezing Point
Boiling Point 278 - 282 °C

@Pressure 0.100 MPa
532 - 540 °F

@Pressure 14.5 psi
Flash Point 144 - 146 °C
291 - 295 °F
Closed Cup
Optical Properties Metric English Comments
Gardner Color Number 1.0 - 4.0
1.0 - 4.0
540MA3C1D
Processing Properties Metric English Comments
Moisture Content 0.00 - 0.10 %
0.00 - 0.10 %
540MA3C74
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear yellow liquid
540MA3C1F
Composition Amine number
0-0.62 mg KOH/g, 540MA3C20