Solvay IGEPAL® CO 660 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name IGEPAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay IGEPAL® CO 660 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHEDCAS: 68412-54-4 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL® CO-660 is an effective emulsifier for nonpolar solvents in solvent emulsion cleaners, dry cleaning detergents.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to Slightly Hazy Liquid
RP-0064
Cloud Point 60-65°C
1% Solution, RP-0124
Color <100
APHA, RP-0134
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343