Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical PB1202 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LG Chemical PB1202 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foaming products by coating, also used for foaming products. It is wide used for products in which plasticizer is rarely added.Main Applications: Synthetic leather, Flooring, Wall coverings, Gloss surface layerCAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.406 g/cc
1.406 g/cc
Bulk Density 0.310 - 0.410 g/cc
0.0112 - 0.0148 lb/in³
ASTM D1895
Volatiles <= 0.30 %

@Temperature 110 °C,
Time 3600 sec
<= 0.30 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 2000 - 6000 cP
2000 - 6000 cP
DOP 60phr; ASTM D1824
Viscosity Measurement >= 2.0
>= 2.0
[g/sec], DOP 60phr, Severs; ASTM D1823
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 1000-1100
30°C, JIS K 6720-2
K-Value 67
DIN53726 / ISO1628-2