Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 25 - 30 µm | 25 - 30 µm | Violet |
30 - 40 µm | 30 - 40 µm | Blue | |
pH | 5.5 - 7.5 | 5.5 - 7.5 | |
Evaporation Loss | <= 1.0 % | <= 1.0 % |
Optical Properties | Metric | English | Comments |
---|---|---|---|
IR Transmittance | 0.00 % @Wavelength 580 nm |
0.00 % @Wavelength 580 nm |
Blue 9:1 |
0.00 % @Wavelength 630 nm |
0.00 % @Wavelength 630 nm |
Blue 9:1 | |
0.00 % @Wavelength 530 nm |
0.00 % @Wavelength 530 nm |
Violet | |
0.00 % @Wavelength 570 nm |
0.00 % @Wavelength 570 nm |
Blue | |
0.00 % @Wavelength 580 nm |
0.00 % @Wavelength 580 nm |
Blue 7:3 | |
0.00 % @Wavelength 580 nm |
0.00 % @Wavelength 580 nm |
Blue 8:2 | |
3.0 % @Wavelength 630 nm |
3.0 % @Wavelength 630 nm |
Blue 8:2 | |
3.0 % @Wavelength 630 nm |
3.0 % @Wavelength 630 nm |
Blue 7:3 | |
3.0 % @Wavelength 680 nm |
3.0 % @Wavelength 680 nm |
Blue | |
5.0 % @Wavelength 780 nm |
5.0 % @Wavelength 780 nm |
Blue | |
10 % @Wavelength 600 nm |
10 % @Wavelength 600 nm |
Violet | |
10 % @Wavelength 630 nm |
10 % @Wavelength 630 nm |
Violet | |
10 % @Wavelength 690 nm |
10 % @Wavelength 690 nm |
Blue 9:1 | |
15 % @Wavelength 780 nm |
15 % @Wavelength 780 nm |
Blue 9:1 | |
20 % @Wavelength 700 nm |
20 % @Wavelength 700 nm |
Blue 8:2 | |
25 % @Wavelength 780 nm |
25 % @Wavelength 780 nm |
Blue 8:2 | |
30 % @Wavelength 380 nm |
30 % @Wavelength 380 nm |
Blue 7:3 | |
30 % @Wavelength 710 nm |
30 % @Wavelength 710 nm |
Blue 7:3 | |
30 % @Wavelength 380 nm |
30 % @Wavelength 380 nm |
Violet | |
30 % @Wavelength 380 nm |
30 % @Wavelength 380 nm |
Blue | |
30 % @Wavelength 380 nm |
30 % @Wavelength 380 nm |
Blue 8:2 | |
30 % @Wavelength 380 nm |
30 % @Wavelength 380 nm |
Blue 9:1 | |
32 % @Wavelength 780 nm |
32 % @Wavelength 780 nm |
Blue 7:3 | |
65 % @Wavelength 440 nm |
65 % @Wavelength 440 nm |
Violet | |
80 % @Wavelength 460 nm |
80 % @Wavelength 460 nm |
Blue 7:3 | |
83 % @Wavelength 460 nm |
83 % @Wavelength 460 nm |
Blue 8:2 | |
87 % @Wavelength 460 nm |
87 % @Wavelength 460 nm |
Blue 9:1 | |
90 % @Wavelength 460 nm |
90 % @Wavelength 460 nm |
Blue | |
95 % @Wavelength 730 nm |
95 % @Wavelength 730 nm |
Violet |
Descriptive Properties | Value | Comments |
---|---|---|
Composition | <100 ppm | Ba |
<300 ppm | Ca | |
Conductivity | <100 µS/cm | Blue |
<100 µS/cm | Violet |