Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name LIMS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesSelective self adhesionNon adhesion to metalsInsert-molding and co-injection molding availableInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
Viscosity 600000 cP
600000 cP
A
600000 cP
600000 cP
B
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength 7.70 MPa
1120 psi
Elongation at Yield 230 %
230 %
Tear Strength 35.0 kN/m
200 pli
Compression Set 10 %

@Temperature 200 °C,
Time 14400 sec
10 %

@Temperature 392 °F,
Time 4.00 hour
40 %

@Temperature 150 °C,
Time 3600 sec
40 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 69
T10 (248°F, ODR)
98
T90 (248°F, ODR)
Regulatory Testing Class VI
Users viewing this material also viewed the following: