Material Notes:
Conformable with: Q/DYS 008-2007TFE Beta-sultone is a colorless transparent liquid. Industrial produced TFE Beta-sultone is mixture of ringlike and straight chain structure, and ringlike structure is transformed into straight chain structure continuously. Owing to its special structure, it is one important fluoride intermediate which can react with various olefines, cycloalkane and nucleophilic reagent.Main Applications:TFE Beta-sultone is one important fluoride intermediate, which can be used to prepare carboxyl and sulfonic group-containing functional compound which are mainly used for functional polymers and fine chemicals, such as PSVE, fluoride surfactant and PFPE.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Density 1.60 g/cc

@Temperature 25.0 °C
0.0578 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 180 g/mol
180 g/mol
Thermal Properties Metric English Comments
Boiling Point 41.0 °C

@Pressure 0.1013 MPa
106 °F

@Pressure 14.69 psi
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
CAS 697-18-7
Chemical Name Tetrafluoroethane Beta-sultone
Danger Label 8 (corrosion)
Molecular Formula C2F4SO3
Purity (%) >95