Material Notes:
Usage: Component of mixture used as refrigerant substituting for CFC-502 and HCFC-22; Fire extinguishing agent substituting for Halon-1211 and Halon-1301Packing: Transport by cylinder or tank, the load index is below 0.9 kg/L. It has to be stored in shady, dry and ventilated place, and avoid exposure to sun and rain.Molecular Formula: C2HF5Structural Formula: CHF2=CF3Conformable with Q/DYG 008-2005Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Density 1.245 g/cc

@Temperature 25.0 °C
0.04498 lb/in³

@Temperature 77.0 °F
Solubility in Water 1.26 %

@Temperature 25.0 °C
1.26 %

@Temperature 77.0 °F
Molecular Weight 120.02 g/mol
120.02 g/mol
Vapor Pressure 13.71 bar

@Temperature 25.0 °C
10280 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 165 J/g
71.0 BTU/lb
at bp
Specific Heat Capacity 0.0900 J/g-°C

@Temperature 25.0 °C
0.0215 BTU/lb-°F

@Temperature 77.0 °F
liquid
Boiling Point -48.45 °C

@Pressure 0.1013 MPa
-55.21 °F

@Pressure 14.69 psi
Chemical Properties Metric English Comments
Critical Pressure 35.92 bar
26940 torr
Critical Temperature 66.05 °C
150.9 °F
Critical Density 0.571 g/cc
0.0206 lb/in³
Acid Value <= 0.10
<= 0.10
HF, mg/kg
Processing Properties Metric English Comments
Moisture Content <= 10 %
<= 10 %
Excellent Grade
<= 20 %
<= 20 %
1st Grade
Descriptive Properties Value Comments
Appearance Colorless
GWP 0.84
Non-Volatile Residue <100
mg/kg
Odor No uncommon odor
ODP 0
Purity (%) >99.5
1st Grade
>99.8
Excellent Grade