Seals Eastern 5724 Fluorocarbon-Elastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Seals Eastern, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 5724 Fluorocarbon-Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.94 g/cc
1.94 g/cc
ASTM D297, 15
Mechanical Properties Metric English Comments
Hardness, Shore A >= 80
>= 80
ASTM D2240, Type A
90
90
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 10.78 MPa
>= 1564 psi
ASTM D412 Method A
14.16 MPa
2054 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 2.38 MPa
>= 345 psi
Stress at Elongation M50; ASTM D412 Method A
2.54 MPa
369 psi
AVG Stress at Elongation M25; ASTM D412 Method A
3.62 MPa
525 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 4.02 MPa
>= 583 psi
Stress at Elongation M100; ASTM D412 Method A
6.09 MPa
884 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 174 %
>= 174 %
ASTM D412 Method A
256 %
256 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.02139 GPa
3.103 ksi
ASTM D412 Method A
Shear Modulus 0.007129 GPa
1.034 ksi
ASTM D412 Method A
Secant Modulus 0.02013 GPa
2.919 ksi
ASTM D412 Method A
Tear Strength Test 258
258
(psi); ASTM D624, Die B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 42