| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D297, 15 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 50 | >= 50 | ASTM D2240, Type A |
| 60 | 60 | AVG; ASTM D2240, Type A | |
| Tensile Strength at Break | >= 10.59 MPa | >= 1536 psi | ASTM D412 Method A |
| 13.64 MPa | 1979 psi | AVG; ASTM D412 Method A | |
| Tensile Strength, Yield | >= 0.0827 MPa | >= 12.0 psi | Stress at Elongation M100; ASTM D412 Method A |
| >= 0.517 MPa | >= 75.0 psi | Stress at Elongation M50; ASTM D412 Method A | |
| 0.752 MPa | 109 psi | AVG Stress at Elongation M25; ASTM D412 Method A | |
| 0.896 MPa | 130 psi | AVG Stress at Elongation M50; ASTM D412 Method A | |
| 1.19 MPa | 173 psi | AVG Stress at Elongation M100; ASTM D412 Method A | |
| Elongation at Break | >= 458 % | >= 458 % | ASTM D412 Method A |
| 778 % | 778 % | AVG; ASTM D412 Method A | |
| Modulus of Elasticity | 0.00511 GPa | 0.741 ksi | ASTM D412 Method A |
| Shear Modulus | 0.00170 GPa | 0.247 ksi | ASTM D412 Method A |
| Secant Modulus | 0.00480 GPa | 0.696 ksi | ASTM D412 Method A |
| Tear Strength Test | 308 | 308 | (psi); ASTM D624, Die B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Strain Energy / Unit Volume at 20% Elongation (psi) | 12 |