Schott Glass 8229 Intermediate sealing glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Schott Glass 8229 Intermediate sealing glass.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Used for sealing to Glass 8228 and Glass 8230 The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.17 g/cc
<br>@Temperature 25.0 °C
0.0784 lb/in³
<br>@Temperature 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 2.00 µm/m-°C
<br>@Temperature 20.0 - 300 °C
1.11 µin/in-°F
<br>@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 600 °C
1110 °F
ISO 7884-8
Softening Point 930.0 °C
1706 °F
Viscosity 10&lt;sup&gt;7.6&lt;/sup&gt; dPa s; ISO 7884-3
Working Point 1440 °C
2624 °F
Viscosity 10&lt;sup&gt;4&lt;/sup&gt; dPa s; ISO 7884-2
Annealing Point 637 °C
1180 °F
Viscosity 10&lt;sup&gt;13&lt;/sup&gt; dPa s; ISO 7884-4
Descriptive Properties Value Comments
tk100(°C) 350
DIN 52326