Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.03 - 1.05 g/cc
1.03 - 1.05 g/cc
Density 0.0139 g/cc
0.000502 lb/in³
Based on 75 times expansion
Bead Size 1.36 - 1.74 mm
0.0535 - 0.0685 in
JIS Z8801
Mechanical Properties Metric English Comments
Flexural Strength 1.80 MPa
261 psi
@ 15 kg/m<sup>2</sup>; ASTM DC201
Compressive Strength >= 0.700 MPa
>= 102 psi
@ 15 kg/m<sup>2</sup>; JIS A9511, ASTM D1621
Chemical Properties Metric English Comments
Blowing Agent Content 6.0 - 7.0 %
6.0 - 7.0 %
Pentane
Descriptive Properties Value Comments
Blocking <1%
Expandability 75 Times
Expansion for 5 min Cheil Method
Fusion >70%
Cheil Method
Polymer Content 93-94%