Saint-Gobain Norton® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam

Category Polymer , Adhesive , Thermoplastic , Vinyl (PVC)
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Low Density Foam Suitable for Sealing of Thin Gauge Metals and Plastics. Closed cell polyvinyl chloride foam sealant with pressure sensitive adhesive on one side. The tight bonding adhesive keeps sealant in place during each stage of product assembly. The adhesive is on the non-linear side, making installation easier and quicker.Features/Benefits:30% compression provides an excellent seal against light, dust and water in mechanically fastened assembliesExcellent resistance to weather, fungi, and oxidation provides a long sealing lifeWill not crack in cold temperaturesSuperb closed cell structure of foam provides a positive sealLow force to compress means faster and easier formation of a positive sealFlexibility facilitates use in radius cornersLow density sealant allows easy assembly of large wall systemsTypical Applications: Curtainwall, precast concrete walls, refridgeration, telecommunications, pheumatic system seals, retail weatherstrip, bus and off-road vehicles, air conditioning, environmentally controlled rooms. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/8" to 1/2".) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.0969 g/cc
0.00350 lb/in³
ASTM D1667
Water Absorption 3.0 %
3.0 %
% by volume; NTP-35
Mechanical Properties Metric English Comments
Hardness, Shore OO 18
18
ASTM D2240
Tensile Strength, Yield 0.117 MPa
17.0 psi
ASTM D-412 (Die A)
Elongation at Break 125 %
125 %
ASTM D-412 (Die A)
Compressive Strength 0.00896 MPa
1.30 psi
Compression Deflection, Compressed to 30%.; ASTM D1667
Compressive Modulus 0.0000138 GPa
0.00200 ksi
Force to Compress, Value for 30% compression.
Compression Set 8.0 %
8.0 %
Constant Deflection, Compressed to 30%.; Norton Test Procedure 37
Thermal Properties Metric English Comments
Thermal Conductivity 0.0389 W/m-K
0.270 BTU-in/hr-ft²-°F
ASTM-C-518
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -26.1 °C
-15.0 °F
Descriptive Properties Value Comments
Color Black