Saint-Gobain Norslide® EKO-V PTFE Sliding Tubing

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Extruded
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norslide®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norslide® EKO-V PTFE Sliding Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features/Benefits:Low stick-slip effectMaintenance free, no lubrication requiredWeatherproofIsolates noise, dampens vibrationFlexible and resilientResistant against fuel, oil, and greasesService temperature range of -328°F to 500°FManufacturing process: Norslide® is high quality sliding tubing made by the paste extrusion method out of PTFE. An emulsion of virgin or filled PTFE fine powder and lubricants is compressed into blanks. These blanks are processed in a paste extruder where they pass a tool which forms the required tubing section. The tubing is then sintered at approximately 350°C to give Norslide® its final strength. Norslide® Compounds: The addition of Saint Gobain Performance Plastic's in-house developed compounds can improve upon the inherent properties of PTFE, particularly its abrasion resistance and specific compression load. The ultimate degree of material alteration will always depend on the application. Applications: Control and selector cables, Accelerator, clutch and brake cables, Parking brake cables, Mirror and air conditioning adjustment, Heating control cables, Hood release cables.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 2.16 g/cc
2.16 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 177 MPa
>= 25600 psi
Elongation at Break >= 275 %
>= 275 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F