Saint-Gobain Fluoroloy® A09 High Performance Seal Material

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Fluoroloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Fluoroloy® A09 High Performance Seal Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Extremely tough, long-wearing material; Excellent in water and water-based fluids, particularly suitable for abrasive media; Long wear life under severe conditions; Limited heat and chemical resistance Information provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Deformation 10 %

@Time 86400 sec
10 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Tensile Modulus 0.531 GPa
77.0 ksi
ASTM D638
Compressive Yield Strength 6.21 MPa

@Strain 1.00 %
901 psi

@Strain 1.00 %
ASTM D695
Compressive Modulus 0.531 GPa
77.0 ksi
ASTM D695
Coefficient of Friction 0.11
0.11
ASTM D3702
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 147 µm/m-°C

@Temperature 26.0 - 200 °C
81.7 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 213 µm/m-°C

@Temperature 26.0 - 200 °C
118 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -268 °C
-450 °F
Descriptive Properties Value Comments
Color Gold