Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufFlex™ GTPE-98-186B PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufFlex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFlex™ GTPE-98-186B PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: A 90°C, dull, PVC alloy jacketing compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60.0

@Time 15.0 sec
60.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 14.1 MPa
2050 psi
ASTM D412
13.536 MPa

@Temperature 121 °C,
Time 605000 sec
1963.2 psi

@Temperature 250 °F,
Time 168 hour
Aged
Elongation at Break 350 %
350 %
ASTM D412
304.5 %

@Treatment Temp. 121 °C,
Time 605000 sec
304.5 %

@Treatment Temp. 250 °F,
Time 168 hour
Aged
Thermal Properties Metric English Comments
Oxygen Index 26.0 %
26.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 177 - 188 °C
350 - 370 °F
Recommended Stock