Material Notes:
Color compound resin available in pellet / powder formKey Characteristics:Excellent stiffnessFair impact resistanceFair processingTypical Applications: High-load/High performance products, such as kayaks, industrial applications, and underground tanksInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D1505
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 1200 %
1200 %
ASTM D368
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
Thermal Properties Metric English Comments
Melting Point 129 °C
264 °F
ASTM D2117
Crystallization Temperature 117 °C
243 °F
ASTM D2117
Descriptive Properties Value Comments
Food Contact Approved FDA
Heavy Metal Free (Base Resin) Yes
Peak Internal Air Temperature 210°C
TPE Method
Shrinkage Level medium
TPE Method
UV Stabilizer UV-8