Material Notes:
15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Melt Flow 6.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
6.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 124 MPa
18000 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 5.03 GPa
730 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 209 MPa
30300 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 5.58 GPa
809 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
4.80 J/cm

@Thickness 3.20 mm
8.99 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 °C

@Thickness 6.40 mm
424 °F

@Thickness 0.252 in
unannealed; ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F