Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics PPO 646 PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name PPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics PPO 646 PPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PPO* 646 resin is a high molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic elastomers like Styrenic Block Copolymers. PPO* resin can be used to improve properties like Heat Distortion and Creep Resistance. It is hydrolytically stable and non-hydroscopic (typically less than 0.2% water uptake). The polymer is soluble in common organic solvents like toluene, chloroform, and THF. Chemical name: Poly (2,6-dimethyl-, 1,4-phenylene ether) (PPE) Formula: (C8H8O)n Regulatory Status: Complies with the FDA regulation 21CFR 177..2460. Also complies with EU Directive 2002/72/EC.
Physical Properties Metric English Comments
Bulk Density 0.465 g/cc
0.0168 lb/in³
ISO 1183
Particle Size 200 µm
200 µm
SABIC Method
Viscosity Measurement 0.46
0.46
Intrinsic Viscosity [dl/g]; SABIC Method
Molecular Weight 68600 g/mol
68600 g/mol
Mw; SABIC Method
Thermal Properties Metric English Comments
Transformation Temperature, Tg 217 °C
423 °F
half width; SABIC Method
Descriptive Properties Value Comments
Mn 21700
SABIC Method
Phenolic End-group Content 820ppm
SABIC Method
Physical Form POWDER
SABIC Method
Toluene Content <1500ppm
SABIC Method