| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded |
| Manufacturer | Radici Group Plastics |
| Trade Name | Heraflex® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Radici Heraflex® P46D 11 I RB T 200 Modified Polypropylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.890 g/cc | 0.890 g/cc |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 46 @Time 3.00 sec |
46 @Time 0.000833 hour |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Minimum Service Temperature, Air | -30.0 °C | -22.0 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |