| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | TIVAR® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
| Water Absorption | <= 0.010 % | <= 0.010 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | <= 0.010 % | <= 0.010 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 65 | 65 | ASTM D2240 |
| Tensile Strength | 40.7 MPa | 5900 psi | ASTM D638 |
| Elongation at Break | 39 % | 39 % | ASTM D638 |
| Tensile Modulus | 0.386 GPa | 56.0 ksi | ASTM D638 |
| Flexural Strength | 20.7 MPa | 3000 psi | ASTM D790 |
| Flexural Modulus | 0.531 GPa | 77.0 ksi | ASTM D790 |
| Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 0.531 GPa | 77.0 ksi | ASTM D695 |
| Izod Impact, Notched | 29.4 J/cm | 55.0 ft-lb/in | ASTM D4020 |
| Coefficient of Friction, Dynamic | 0.090 | 0.090 | Dry vs. Steel; QTM55007 |
| Sand Slurry | 16.5 | 16.5 | 1018 Steel = 100 |
| Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 144 µm/m-°C @Temperature -40.0 - 149 °C |
80.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1e+14 ohm | >= 1e+14 ohm | ASTM D257 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Sand Water Wheel | 101 | ASTM G65; TIVAR® 1000 = 100 |