Precision Polymer Engineering S50K Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering S50K Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. Formulated to BS2494 Type ‘W’ and Water Research Council (WRC) tested in accordance with BS6920 ‘Items which have passed full tests of effects on water quality’ (for use in potable water applications). ASTM & ISO designation = VMQ. WRC Approval No. 9910521.Applications: Cold and hot water, plus low pressure steam, up to +110°C.
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
°IRHD; ASTM D1415
45 - 55
45 - 55
°IRHD, ±5 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D412
7.20 - 10.8 MPa
1040 - 1570 psi
±20% change after 168 hours @ 70°C; ASTM D412
Elongation at Break 375 %
375 %
ASTM D412
262.5 - 487.5 %
262.5 - 487.5 %
±30% change after 168 hours @ 70°C; ASTM D412
Compression Set 12 %
12 %
70 hours @ 23°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F