| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA) | 
| Manufacturer | Arkema | 
| Trade Name | Pebax® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Conditioned).pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.01 g/cc | 0.0365 lb/in³ | |
| Melt Flow |           8.0           g/10 min           @Load 1.00 kg, Temperature 235 °C  | 
                  8.0           g/10 min           @Load 2.20 lb, Temperature 455 °F  | 
        
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D | 55 | 55 | |
| Tensile Strength, Yield | 12.0 MPa | 1740 psi | 50 mm/min | 
| Elongation at Break | >= 50 % | >= 50 % | Nominal Strain; 50 mm/min | 
| Elongation at Yield | 31 % | 31 % | 50 mm/min | 
| Tensile Modulus | 0.150 GPa | 21.8 ksi | 1 mm/min | 
| Charpy Impact Unnotched | NB | NB | |
| NB | NB | Low Temp | |
| Charpy Impact, Notched | NB | NB | |
| NB | NB | Low Temp | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow |           170           µm/m-°C           @Temperature 20.0 °C  | 
                  94.4           µin/in-°F           @Temperature 68.0 °F  | 
        |
| Melting Point | 159 °C | 318 °F | (Dry) | 
| Deflection Temperature at 0.46 MPa (66 psi) | 66.0 °C | 151 °F | |
| Vicat Softening Point | 144 °C | 291 °F | 50°C/hr; 50N | 
| Flammability, UL94 |           HB                     @Thickness 1.60 mm  | 
                  HB                     @Thickness 0.0630 in  | 
        
| Optical Properties | Metric | English | Comments | 
|---|---|---|---|
| Transmission, Visible | 80 % | 80 % | Mfr. reports 'Transparent' but doesn't quantify. | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm |