PolyOne Nymax™ GF1800-40 HS Black 13 Nylon 6/12, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ GF1800-40 HS Black 13 Nylon 6/12, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description/Features:Glass Fiber ReinforcedHeat StabilizedNylon 6/12 CompoundBlackDry as molded:PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 162 MPa
23500 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus 9.51 GPa
1380 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
Unannealed; ASTM D648