PolyOne Maxxam™ FR PE 112 LDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne Maxxam™ FR PE 112 LDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.
Physical Properties Metric English Comments
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
0.980 g/cc
0.980 g/cc
ASTM D792
Melt Flow 9.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.1 MPa
2050 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 500 %
500 %
Type I, 51 mm/min; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
Flammability, UL94 V-2

@Thickness 1.59 mm
V-2

@Thickness 0.0626 in
NC; UL 94
Oxygen Index 25 %

@Thickness 3.18 mm
25 %

@Thickness 0.125 in
ASTM D2863
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Name Polyethylene, Low Density (LDPE)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America