Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 200 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 392 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.9 MPa
9990 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 4.41 GPa
640 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.41 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
BK; UL 94
Processing Properties Metric English Comments
Mold Temperature 16.0 - 50.0 °C
60.8 - 122 °F
Descriptive Properties Value Comments
Appearance Black
Features General Purpose
Filler / Reinforcement GlassMineral
Unspecified FillerReinfor., 30% Filler by Weight
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Consumer Applications
General Purpose
Industrial Applications