PolyOne Geon™ Vinyl Flexible A90F1 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible A90F1 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Recommended for interior applications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 sec; ASTM D2240
90
90
ASTM D2240
Tensile Strength at Break 17.9 MPa
2600 psi
510 mm/min; ASTM D638
Tensile Strength 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
510 mm/min; ASTM D638
Tear Strength 87.6 kN/m
500 pli
Die C, 510 mm/min; ASTM D624
Clash Berg Modulus 0.565 GPa
81.9 ksi
ASTM D1043
0.310 GPa

@Temperature -23.0 °C
45.0 ksi

@Temperature -9.40 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -27.8 °C
-18.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 80.6 - 83.3 °C
177 - 182 °F
Descriptive Properties Value Comments
Additive Biocide
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications