Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
15 sec; ASTM D2240
Tensile Strength at Break 10.2 MPa
1480 psi
510 mm/min; ASTM D638
Elongation at Break 440 %
440 %
510 mm/min; ASTM D638
Tear Strength 26.2 kN/m
149 pli
Die C, 2 in/min; ASTM D1004
Descriptive Properties Value Comments
Automotive Specifications FORD ESB-M4D259 Type I
FORD ESB-M4D284 Type I
FORD ESB-M4D284-C1 Color: Black
Features General Purpose
Low Gloss
Forms Pellets
Fungal Resistance Pass
ASTM G21
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Low Temperature Flexibility Pass
-29°C, 508.0 µm; 4 hr, 12 mm
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
General Purpose
Outdoor Applications
Xenon Weatherometer Pass
SAE J1960; Exterior, 2500 kJ/m², Black, dE*<3.0