Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne FireCon™ CPE 37-11 RoHS BLACK Polyethylene, Chlorinated (CPE)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer PolyOne Corporation
Trade Name FireCon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne FireCon™ CPE 37-11 RoHS BLACK Polyethylene, Chlorinated (CPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CPE-37-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-37-11 RoHS BLACK offers the highest physical properties and flexibility, great surface quality, good heat shock resistance as well as ease of processing on large cables..Note: Pre-drying is recommended for 4 hours at 175°-185°F. Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment. NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
10 sec; ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.00689 GPa
0.999 ksi
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Oxygen Index 31 %

@Thickness 1.91 mm
31 %

@Thickness 0.0752 in
ASTM D2863
Descriptive Properties Value Comments
Appearance Pellets/Cubes
ASTM D2090
Forms Pellets
Generic Material CPE
Generic Name Polyethylene, Chlorinated (CPE)
Regional Availability Asia Pacific
North America
South America
RoHS Compliance RoHS Compliant
Uses Cable Jacketing
Wire & Cable Applications
Copyright © lookpolymers.com All Rights Reserved