Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Piezo Kinetics 532 Lead Zirconate Titanate Piezoelectric

Category Ceramic , Oxide , Titanium Oxide , Zirconium Oxide , Piezoelectric
Manufacturer Piezo Kinetics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Piezo Kinetics 532 Lead Zirconate Titanate Piezoelectric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Denoted as Navy Type V, this ceramic is used as sensors that require low impedance, high dielectric constant and high sensitivity.Elastic Compliance s11E (x 10-12 m²/n): 15.9.Elastic Compliance s33E (x 10-12 m²/n): 18.Property data at 25°C. Information supplied by Piezo Kinetics, Inc.
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 63.0 GPa
9140 ksi
Poissons Ratio 0.31
0.31
Shear Modulus 24.0 GPa
3480 ksi
calculated
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Maximum Operating Temperature
Electrical Properties Metric English Comments
Curie Temperature 220 °C
428 °F
Dielectric Constant 2700

@Frequency 1000 Hz
2700

@Frequency 1000 Hz
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.70
0.70
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -230
-230
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 670
670
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 20.5
20.5
Piezoelectric Planar Coupling Factor, kp 0.63
0.63
Piezoelectric Mechanical Q 75
75
Piezoelectric Shear Coupling Factor, k15 0.67
0.67
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 490
490
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -9.60
-9.60
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 28
28
Piezoelectric Transverse Coupling Factor, k31 0.36
0.36
Users viewing this material also viewed the following: