Pau Tai UNISTAB EC-298 Stabilizers for Cable

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name UNISTAB
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai UNISTAB EC-298 Stabilizers for Cable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent electrical insulation and heat endurance. Use level depends on lacked products, general:3-7PHR. EC-198 specially applicable to preparations with high filling content.Information provided by Pau Tai Industrial Corp.