Parker Chomerics Tecknit® 72-00005 Silver-Filled Flexible Resin Caulking System

Category Polymer
Manufacturer Parker Chomerics
Trade Name Tecknit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit® 72-00005 Silver-Filled Flexible Resin Caulking System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide over 100 dB total shielding effectiveness across the RF spectrum. They may be used to improve joint or seam integrity for all types of electronic enclosures. An outstanding feature of these one-component systems is the ease with which they may be applied with conventional caulking guns and dispensing equipment, such as small bead orifice syringes. Hand application with spatula or putty knife is also simple. High yield per pound is another advantage offered in these conductive caulks. Proprietary formulation techniques result in lower density than most current state-of-the-art caulking compounds. The systems are safe to handle, very easily applied and free of any corrosive binders. They contain silver plated glass or copper particles for electrical conductivity, assuring stable operation over wide temperature ranges not generally possible with carbon- black filled systems.Application Information: This thixotropic cream system, which remains permanently flexible after curing, is easy to apply with standard caulking equipment. It is a thermoplastic + solvent type, which dries quickly to a highly conductive seal. Small beads are easily drawn. It is safe to handle, nonexothermic and has excellent adhesion to metal. The system is watertight, ozone resistant, andnon-corrosive to applied surfaces. Among the chief uses are caulking EMI tight cabinets and enclosures, fasteners, panels and handles. The system is extremely vibration and thermal shock resistant.Information provided by Chomerics
Mechanical Properties Metric English Comments
Shear Strength >= 0.0276 MPa
>= 4.00 psi
Cured; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 94.0 °C
201 °F
Cured
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Cured
Shrinkage <= 46 %
<= 46 %
Cured
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Cured; QAP-1017
Processing Properties Metric English Comments
Cure Time 4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Recommended Cure
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Full Cure
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Descriptive Properties Value Comments
Color Tan
Consistency Liquid
Filler Ag/Glass
Final Condition Flexible
Number of Components One
Resin Polyolefin
Volume 16 in3
Weight 16 oz