Material Notes:
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.High hardness with corrosion resistance of 400 series stainless steels. Magnetic.Ferro-TiC® Unique CharacteristicsProvides the lightweight, size, stability, and hardnessVirtually porosity free - significantly better than the A1 ASTM B-276-79 StandardLow specific mass. Ferro-Tic® is 10-20% lighter than its steel counterpart and about 50% lighter than tungsten carbide10 times the wear resistance of tool steelsEconomical fabrication (conventionally machinable in the annealed stage by milling and turning, conventionally heat treatable to achieve high hardness)50-90% less linear size change in heat treat than tool steelsInformation Provided by Ferro-TiC®, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.45 g/cc
0.233 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 50
50
Annealed
68
68
Hardened
Flexural Strength 1030 MPa
149000 psi
Transverse Rupture
Compressive Strength 3120 MPa
453000 psi
Charpy Impact Unnotched 2.589 J/cm²
12.33 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear 4.41 µm/m-°C

@Temperature 21.1 - 371 °C
2.45 µin/in-°F

@Temperature 70.0 - 700 °F
Maximum Service Temperature, Air 371 °C
700 °F
Descriptive Properties Value Comments
Carbide (Vol. %) 45
Linear Size Change Thru Heat Treat % 0.016
Thermal Shock (No. Cycles) 1