Material Notes:
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a HP4294A.
Physical Properties Metric English Comments
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
Particle Size 120 µm
120 µm
median granule size
Thermal Properties Metric English Comments
Shrinkage 15.5 %
15.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 1e+8 ohm-cm
1e+8 ohm-cm
Magnetic Coercive Force, Hc 0.45 Oe
0.45 Oe
Magnetic Remanence, Br 2100 Gauss
2100 Gauss
Curie Temperature 160 °C
320 °F
Processing Properties Metric English Comments
Moisture Content 0.30 %
0.30 %
Sintering Temperature 1220 °C

@Time 7200 sec
2230 °F

@Time 2.00 hour
Descriptive Properties Value Comments
Flux Density Bs 3500 Gauss
Field Strength = 30 Oe
Initial Permeability, µi 860
Q Factor (w/ 10 turns) 50
0.1 MHz
Users viewing this material also viewed the following: