Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers OPX782 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Bead Filled
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers OPX782 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
380 °F
ASTM D648
Users viewing this material also viewed the following: