Nye Lubricants UniFlor 8110 (UF) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Nye Lubricants
Trade Name UniFlor
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants UniFlor 8110 (UF) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 105
105
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 25 cSt
25 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.7 cSt
4.7 cSt
Base Oil; ASTM D445
Evaporation Loss 25 %
25 %
24 hrs, 150C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Recommended
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Recommended
Pour Point -56.0 °C
-68.8 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(pnd)